Fábrica de herramientas de fresado y corte sdftools

SDF-NS Series Solid carbide 5-flute square end mill for high-temperature alloys and titanium alloys

Rated 5.00 out of 5 based on 1 customer rating
(1 customer review)
  • Unique 5-flute design ensures high metal removal rates, suitable for both roughing and semi-finishing operations.
  • Advanced ALTIN coating process significantly enhances tool wear resistance and anti-adhesion properties, extending tool life and improving surface finish.
  • Manufactured from high-quality fine-grain micro-particle solid carbide material, ensuring high hardness and toughness, capable of machining materials with hardness up to HRC 60°.
  • Precision ground on advanced German WALTER five-axis grinders, ensuring geometric accuracy and surface quality, guaranteeing consistent performance and tight tolerances.
  • Inspected using German ZOLLER measuring equipment, ensuring high and stable tool quality.
ico/流程/技术
Máxima rentabilidad a igual calidad
ico/流程/生产配送
Amplio stock, envío en 1-2 días
ico/流程/生产优化
Un equipo profesional orienta en el corte
ico/流程/持续优化
Devoluciones/cambios gratuitos si el corte de prueba no es satisfactorio

 

Características








Aplicaciones








Materiales de trabajo




SDF-NS Series 5-Flute Solid Carbide End Mill

Material

  1. High-Quality Fine-Grain Micro-Particle Solid Carbide Material:
    • Manufactured from high-quality fine-grain micro-particle solid carbide material, ensuring high hardness and toughness, capable of machining materials with hardness up to HRC 60°.

Design

  1. Unique 5-Flute Design:
    • Unique 5-flute design ensures high metal removal rates, suitable for both roughing and semi-finishing operations.
  2. Advanced ALTIN Coating Process:
    • Advanced ALTIN (Aluminum Titanium Nitride) coating process significantly enhances tool wear resistance and anti-adhesion properties, extending tool life and improving surface finish.

Functions

  1. High Metal Removal Rates:
    • The 5-flute design enables high metal removal rates, making it ideal for roughing operations where large amounts of material need to be removed quickly.
  2. Smooth Chip Evacuation:
    • The design ensures smooth chip evacuation, reducing the risk of chip clogging and improving machining efficiency.
  3. Excellent Wear Resistance and Anti-Adhesion Properties:
    • The ALTIN coating provides superior wear resistance and anti-adhesion properties, extending the tool’s life and improving the surface finish of the workpiece.
  4. High Hardness and Toughness:
    • The high-quality fine-grain micro-particle solid carbide material ensures the tool can handle materials with hardness up to HRC 60°, making it suitable for a wide range of applications.
  5. Geometric Accuracy and Surface Quality:
    • Precision grinding on advanced German WALTER five-axis grinders ensures geometric accuracy and surface quality, guaranteeing consistent performance and tight tolerances.

Aplicaciones

  1. Superalloys and Titanium Alloys:
    • Primarily designed for semi-finishing operations on superalloys and titanium alloys, which are commonly used in the aerospace, automotive, and energy sectors.
  2. Roughing and Semi-Finishing Operations:
    • Suitable for both roughing and semi-finishing operations, providing versatility in various machining processes.
  3. High-Precision Parts:
    • The high geometric accuracy and surface quality make the tool ideal for machining high-precision parts, such as those used in aerospace and medical device manufacturing.
  4. Thin-Wall and Complex Components:
    • The smooth chip evacuation and reduced vibration make the tool suitable for machining thin-wall and complex components, ensuring dimensional accuracy and surface finish.
Revestimiento

ALTIN Coat

Recuento de flautas

5 Flutes

Tipo de flauta

Fresa

HRC

HRC60°

Material a mecanizar

Dimensions

Número de pedidoEspecificaciónNumber
of Flutes
T
Corte
Diámetro
Φ
Corte
Longitud
H2
Clearance
Longitud
H1
Vástago
Diámetro
D
En general
Longitud
L
MNS51565ASH-41220Y650Φ4*12*50*D6541220650
MNS51565ASH-51523Y650Φ5*15*50*D6551523650
MNS51565ASH-61826Y650Φ6*18*50*D6561826650
MNS51565ASH-82432Y860Φ8*24*60*D8582432860
MNS51565ASH-103038Y1075Φ10*30*75*D1051030381075
MNS51565ASH-123644Y1275Φ12*36*75*D1251236441275
MNS51565ASH-164856Y16100Φ16*48*100*D16516485616100
MNS51565ASH-185462Y18100Φ18*54*100*D18518546218100
MNS51565ASH-205462Y20100Φ20*54*100*D20520546220100

1 review for SDF-NS Series Solid carbide 5-flute square end mill for high-temperature alloys and titanium alloys

  1. Rated 5 out of 5

    admin

    good

Add a review

PREGUNTAS FRECUENTES

Nuestra fábrica se encuentra en Wuhan, China, y está especializada en fresas y brocas de gama media-alta. Damos la bienvenida a las visitas in situ.

  1. 首先,我们确定您的要求。我们的工程师将与您沟通以了解您的需求。
  2. 一旦需求得到确认,我们将创建工具图纸。
  3. 在您批准图纸后,我们将安排生产。
  4. 最后,我们将交付测试工具。

Aceptamos los métodos de pago más habituales. Los acuerdos específicos pueden ser discutidos con nuestro gerente de ventas para encontrar un método conveniente para ambas partes.

Admitimos cantidades mínimas de pedido para las pruebas. Si la calidad no cumple nuestro compromiso de venta, ofrecemos devoluciones gratuitas y cubrimos los gastos de envío.

Normalmente utilizamos el envío rápido. La entrega en todo el mundo tarda entre 7 y 15 días. Si se utiliza el transporte aéreo de FedEx, puede acortarse a entre 3 y 5 días.

Estamos especializados en personalización no estándar y gestionamos un gran volumen de pedidos personalizados a diario, resolviendo la mayoría de los problemas. Cuando envíe su formulario, márquelo como "personalización no estándar" y un ingeniero especializado en herramientas se pondrá en contacto con usted.

Por supuesto. Contamos con ingenieros de herramientas e ingenieros de aplicaciones experimentados, y tenemos numerosos casos prácticos de soluciones integrales. Sin embargo, debido a la larga distancia, sólo podemos ayudar a los distribuidores locales a aplicar estas soluciones integrales.

我们的工程师在新加坡拥有16年的工具定制经验,可以流利地用中英文沟通。

Póngase en contacto con nosotros

Ir arriba

Get a fast response from our expert

Personalice

Rellene sus necesidades de personalización,Nuestros ingenieros le responderán dentro de 12 horas.