SDF-N Series Solid Carbide Difficult-to-Machine Materials 4-flute ball nose end mill for machining superalloys, titanium alloys

  • 2-Flute design with large chip clearance grooves, reducing chip clogging and improving machining efficiency.
  • Specialized PT coating material effectively reduces tool adhesion, extending tool life and improving workpiece surface quality.
  • Made from fine-grain micro-particle substrate, ensuring tool stability and high milling performance.
  • Suitable for difficult-to-machine materials such as superalloys and titanium alloys.
ico/流程/技术
Highest cost-performance for equal quality
ico/流程/生产配送
Ample stock, shipped within 1-2 days
ico/流程/生产优化
Professional team offers cutting guidance
ico/流程/持续优化
Free returns/exchanges if trial cutting is unsatisfactory

 

Features








Applications








Work Materials




Product Description

Product Design

  1. 2-Flute Ball Nose End Mill:2-Flute ball nose end mill design with large chip clearance grooves ensures efficient chip evacuation, reduces chip clogging, and improves machining efficiency.
  2. Fine-Grain Micro-Particle Substrate:Made from fine-grain micro-particle substrate to ensure tool stability and high milling performance.

Coating Material

  1. Specialized PT Coating Material:Specialized PT coating material effectively reduces tool adhesion, extends tool life, and improves workpiece surface quality.

Function

  1. High Efficiency:Optimized for high-efficiency machining of superalloys and titanium alloys, with advanced tool geometry and coating technology ensuring efficient cutting in hard materials.
  2. Stability and Reliability:Provides stable and reliable performance, ensuring consistent quality and precision in demanding applications.

Suitable Milling Methods

  1. Suitable for Side Milling and Contour Milling:Particularly suitable for side milling and contour milling, capable of accurately machining complex 3D surfaces and side walls, ensuring surface finish and precision.
  2. Can Also Be Used for Slot Milling:Can also be used for slot milling, suitable for deep and narrow slots, ensuring good chip evacuation and stable cutting performance.

Application Scenarios

  1. Aerospace, Mold Manufacturing, and Other High-Demand Industries:Widely used in high-demand industries such as aerospace and mold manufacturing, suitable for difficult-to-machine materials like superalloys and titanium alloys.
Flute Type

Ball End Mill

Coating

PT Coat

Flute Count

2 Flutes

Material to be Machined

Dimensions

Order NumberSpecificationNumber
of Flutes
Arc
Radius
Cutting
Length
Shank
Diameter
Overall
Length
TRHDL
MN92265ASH-0102N450R0.1*0.2*50*D420.10.2450
MN92265ASH-01503N450R0.15*0.3*50*D420.150.3450
MN92265ASH-0204N450R0.2*0.4*50*D420.20.4450
MN92265ASH-02506N450R0.25*0.6*50*D420.250.6450
MN92265ASH-0309N450R0.3*0.9*50*D420.30.9450
MN92265ASH-0412N450R0.4*1.2*50*D420.41.2450
MN92265ASH-0515N450R0.5*1.5*50*D420.51.5450
MN92265ASH-07523N450R0.75*2.3*50*D420.752.3450
MN92265ASH-103N450R1.0*3*50*D4213450
MN92265ASH-1545N450R1.5*4.5*50*D421.54.5450
MN92265ASH-206N450R2.0*6*50*4D226450
MN92265ASH-206N475R2.0*6*75*4D226475
MN92265ASH-206N4100R2.0*6*100*4D2264100
MN92265ASH-103N650R1.0*3*50*D6213650
MN92265ASH-1545N650R1.5*4.5*50*D621.54.5650
MN92265ASH-208N650R2.0*8*50*D6228650
MN92265ASH-2575N650R2.5*7.5*50*D622.57.5650
MN92265ASH-309N650R3.0*9*50*D6239650
MN92265ASH-309N660R3.0*9*60*D6239660
MN92265ASH-309N675R3.0*9*75*D6239675
MN92265ASH-309N6100R3.0*9*100*D62396100
MN92265ASH-4012N860R4.0*12*60*D82412860
MN92265ASH-4012N875R4.0*12*75*D82412875
MN92265ASH-4012N8100R4.0*12*100*D824128100
MN92265ASH-4012N8150R4.0*12*150*D824128150
MN92265ASH-5015N1075R5.0*15*75*D1025151075
MN92265ASH-5015N10100R5.0*15*100*D10251510100
MN92265ASH-5015N10150R5.0*15*150*D10251510150
MN92265ASH-6018N1275R6.0*18*75*D1226181275
MN92265ASH-6018N12100R6.0*18*100*D12261812100
MN92265ASH-6018N12150R6.0*18*150*D12261812150
MN92265ASH-728N14100R7*28*100*D14272814100
MN92265ASH-728N14150R7*28*150*D14272814150
MN92265ASH-832N16100R8*32*100*D16283216100
MN92265ASH-832N16150R8*32*150*D16283216150
MN92265ASH-1040N20100R10*40*100*D202104020100
MN92265ASH-1040N20150R10*40*150*D202104020150

Avaliações

Ainda não existem avaliações.

Seja o primeiro a avaliar “SDF-N Series Solid Carbide Difficult-to-Machine Materials 4-flute ball nose end mill for machining superalloys, titanium alloys”

FAQ

Our factory is located in Wuhan, China, specializing in mid-to-high-end milling cutters and drills. We welcome on-site visits.

  1. 首先,我们确定您的要求。我们的工程师将与您沟通以了解您的需求。
  2. 一旦需求得到确认,我们将创建工具图纸。
  3. 在您批准图纸后,我们将安排生产。
  4. 最后,我们将交付测试工具。

We accept most common payment methods. Specific arrangements can be discussed with our sales manager to find a convenient method for both parties.

We support minimum order quantities for trials. If the quality does not meet our sales commitment, we offer free returns and cover shipping costs.

We typically use fast shipping. Delivery globally takes about 7 to 15 days. If using FedEx air freight, it can be shortened to 3 to 5 days.

We specialize in non-standard customization and handle a large volume of custom orders daily, solving most issues. When submitting your form, please mark it as “non-standard customization,” and a dedicated tool engineer will contact you.

Of course. We have experienced tool engineers and application engineers, and we have numerous case studies of comprehensive solutions. However, due to the long distance, we can only assist local distributors in implementing these comprehensive solutions.

我们的工程师在新加坡拥有16年的工具定制经验,可以流利地用中英文沟通。

Contact Us

Deslocar para o topo

Get a fast response from our expert

Personalizar

Preencha suas necessidades de personalização , Nossos engenheiros responderão a você dentro de 12 horas.