SDF-N Series Solid Carbide Difficult-to-Machine Materials 4-flute radius end mill for machining superalloys, titanium alloys

  • Unique cutting edge geometry design, specifically tailored for machining superalloys, titanium alloys, and other difficult-to-machine materials.
  • Advanced PT coating process, significantly enhancing tool wear resistance and anti-adhesion properties, extending tool life and improving surface finish.
  • Manufactured from high-quality fine-grain micro-particle solid carbide material, ensuring high hardness and toughness of the tool.
  • Precision ground on advanced German WALTER five-axis grinders, ensuring geometric accuracy and surface quality, guaranteeing consistent performance and tight tolerances.
  • Inspected using German ZOLLER measuring equipment, ensuring high and stable tool quality.
ico/流程/技术
Высочайшая экономичность при равном качестве
ico/流程/生产配送
Большой запас, доставка в течение 1-2 дней
ico/流程/生产优化
Профессиональная команда предлагает руководство по резке
ico/流程/持续优化
Бесплатный возврат/обмен при неудовлетворительном результате пробной резки

 

Характеристики








Приложения








Материалы для работы




SDF-N Series 4-Flute Radius End Mill for Superalloys and Titanium Alloys

Overall Design Features

  1. Unique Cutting Edge Geometry Design:Unique cutting edge geometry design specifically tailored for machining superalloys, titanium alloys, and other difficult-to-machine materials, ensuring efficient cutting performance and long tool life.
  2. Advanced PT Coating Process:Advanced PT coating process significantly enhances tool wear resistance and anti-adhesion properties, extending tool life and improving workpiece surface finish.
  3. High-Quality Fine-Grain Micro-Particle Solid Carbide Material:Manufactured from high-quality fine-grain micro-particle solid carbide material, ensuring high hardness and toughness, providing stable performance under extreme conditions.
  4. Precision Ground on Advanced German WALTER Five-Axis Grinders:Precision ground on advanced German WALTER five-axis grinders, ensuring geometric accuracy and surface quality, guaranteeing consistent performance and tight tolerances.
  5. Inspected Using German ZOLLER Measuring Equipment:Inspected using German ZOLLER measuring equipment, ensuring high and stable tool quality.

Suitable Milling Methods

  1. Side Milling and Contour Milling:Particularly suitable for side milling and contour milling, capable of accurately machining complex 3D surfaces and side walls, ensuring surface finish and precision.
  2. Slot Milling:Can also be used for slot milling, suitable for deep and narrow slots, ensuring good chip evacuation and stable cutting performance.
  3. High-Efficiency Milling:Ideal for high-efficiency milling, especially in the machining of complex parts requiring high precision and stability, significantly improving production efficiency.

Application Scenarios

  1. Aerospace Industry:Widely used in the aerospace industry for machining aircraft engine components, structural parts, and other superalloy and titanium alloy materials.
  2. Производство пресс-форм:Used in mold manufacturing for machining high-precision molds, ensuring surface quality and dimensional accuracy.
  3. Medical Device Manufacturing:Used in medical device manufacturing for machining precision medical devices, ensuring reliability and safety of the products.
  4. Automotive Industry:Used in the automotive industry for machining high-performance parts such as turbocharger blades and engine blocks.
  5. Energy Sector:Used in the energy sector for machining critical components of nuclear power, wind power, and other equipment, ensuring long-term stable operation of the equipment.
Покрытие

PT Coat

Флейта

4 флейты

HRC

HRC60°

Тип флейты

Cor Radius End mill

Обрабатываемый материал

Размеры изделия

Номер заказаТехнические характеристикиNumber
of Flutes
Резка
Диаметр
Arc
Radius
Резка
Длина
Хвостовик
Диаметр
В целом
Длина
TΦRHDL
MN93465ASH-1023N450Φ1*R0.2*3*50*D4410.23450
MN93465ASH-15024N450Φ1.5*R0.2*4*50*D441.50.24450
MN93465ASH-2026N450Φ2*R0.2*6*50*D4420.26450
MN93465ASH-25028N450Φ2.5*R0.2*8*50*D442.50.28450
MN93465ASH-25058N450Φ2.5*R0.5*8*50*D442.50.58450
MN93465ASH-3028N450Φ3*R0.2*8*50*D4430.28450
MN93465ASH-3058N450Φ3*R0.5*8*50*D4430.58450
MN93465ASH-40210N450Φ4*R0.2*10*50*D4440.210450
MN93465ASH-40510N450Φ4*R0.5*10*50*D4440.510450
MN93465ASH-50213N650Φ5*R0.2*13*50*D6450.213650
MN93465ASH-50513N650Φ5*R0.5*13*50*D6450.513650
MN93465ASH-5113N650Φ5*R1*13*50*D645113650
MN93465ASH-60315N650Φ6*R0.3*15*50*D6460.315650
MN93465ASH-60515N650Φ6*R0.5*15*50*D6460.515650
MN93465ASH-6115N660Φ6*R1*15*50*D646115660
MN93465ASH-80320N860Φ8*R0.3*20*60*D8480.320860
MN93465ASH-80520N860Φ8*R0.5*20*60*D8480.520860
MN93465ASH-8120N860Φ8*R1*20*60*D848120860
MN93465ASH-100325N1075Φ10*R0.3*25*75*D104100.3251075
MN93465ASH-100525N1075Φ10*R0.5*25*75*D104100.5251075
MN93465ASH-10125N1075Φ10*R1*25*75*D104101251075
MN93465ASH-10225N1075Φ10*R2*25*75*D104102251075
MN93465ASH-120330N1275Φ12*R0.3*30*75*D124120.3301275
MN93465ASH-120530N1275Φ12*R0.5*30*75*D124120.5301275
MN93465ASH-12130N1275Φ12*R1*30*75*D124121301275
MN93465ASH-12230N1275Φ12*R2*30*75*D124122301275
MN93465ASH-160345N16100Φ16*R0.3*45*100*D164160.34516100
MN93465ASH-160545N16100Φ16*R0.5*45*100*D164160.54516100
MN93465ASH-16145N16100Φ16*R1.0*45*100*D1641614516100
MN93465ASH-16245N16100Φ16*R2.0*45*100*D1641624516100
MN93465ASH-180345N18100Φ18*R0.3*45*100*D184180.34518100
MN93465ASH-180545N18100Φ18*R0.5*45*100*D184180.54518100
MN93465ASH-18145N18100Φ18*R1.0*45*100*D1841814518100
MN93465ASH-18245N18100Φ18*R2.0*45*100*D1841824518100
MN93465ASH-200345N20100Φ20*R0.3*45*100*D204200.34520100
MN93465ASH-200545N20100Φ20*R0.5*45*100*D204200.54520100
MN93465ASH-20145N20100Φ20*R1.0*45*100*D2042014520100
MN93465ASH-20245N20100Φ20*R2.0*45*100*D2042024520100

видео

Отзывы

Отзывов пока нет.

Будьте первым, кто оставил отзыв на "SDF-N Series Solid Carbide Difficult-to-Machine Materials 4-flute radius end mill for machining superalloys, titanium alloys"

ЧАСТО ЗАДАВАЕМЫЕ ВОПРОСЫ

Наш завод находится в городе Ухань, Китай, и специализируется на производстве фрез и сверл среднего и высокого класса. Мы приглашаем вас посетить наш завод.

  1. 首先,我们确定您的要求。我们的工程师将与您沟通以了解您的需求。
  2. 一旦需求得到确认,我们将创建工具图纸。
  3. 在您批准图纸后,我们将安排生产。
  4. 最后,我们将交付测试工具。

Мы принимаем большинство распространенных способов оплаты. Конкретные условия можно обсудить с нашим менеджером по продажам, чтобы подобрать удобный для обеих сторон способ.

Мы поддерживаем минимальное количество заказов для испытаний. Если качество не соответствует нашим обязательствам, мы предлагаем бесплатный возврат и оплачиваем стоимость доставки.

Как правило, мы используем быструю доставку. Доставка по всему миру занимает от 7 до 15 дней. При использовании авиаперевозки FedEx этот срок может быть сокращен до 3-5 дней.

Мы специализируемся на нестандартных заказах и ежедневно выполняем большой объем заказов, решая большинство проблем. При отправке формы пометьте ее как "нестандартный заказ", и с вами свяжется инженер-инструментальщик.

Конечно. У нас есть опытные инженеры-инструментальщики и инженеры по применению, и мы располагаем многочисленными примерами комплексных решений. Однако из-за большого расстояния мы можем помочь местным дистрибьюторам в реализации этих комплексных решений.

我们的工程师在新加坡拥有16年的工具定制经验,可以流利地用中英文沟通。

Свяжитесь с нами

滚动至顶部

Get a fast response from our expert

Настроить

Наши инженеры ответят вам в течение 12 часов.